| Brand Name: | YUHONG |
| Model Number: | ASTM A213 TP316L Stainless Steel Coiled Tube |
| MOQ: | 1000kgs |
| Packaging Details: | Ply-wooden Case /Iron Case/ Bundle with plastic Cap |
| Payment Terms: | L/C,T/T |
ASTM A213 TP316L Stainless Steel Seamless Coil Tube Heat Exchanger Tubing in Coil
This is a cold-drawn, seamless austenitic stainless tube made to ASTM A213 / ASME SA213 in grade TP316L (UNS S31603) and delivered in coil form rather than straight lengths. The material is the low-carbon, molybdenum-bearing grade of the 316 family: 16–18 % chromium, 10–14 % nickel and 2.00–3.00 % molybdenum, with carbon held at 0.035 % maximum. It is chosen for one reason above all others — it has to carry a heat-transfer duty inside equipment that cannot be opened for repair, so the tube wall must resist both the process side and the cooling side at the same time, and it must survive being formed into a coil without losing that resistance.
Coiling changes the engineering problem completely. A straight tube bought in 6 m lengths has to be cut, welded and flanged into a serpentine on site; every weld is a future leak path, every butt joint needs radiography or at least dye-penetrant inspection, and the assembly has to be heat-treated or accepted with residual stress in the bends. A single continuous coil arrives with the geometry already built in: the tube runs from inlet to outlet without an intermediate joint, wall thinning in the bend is controlled by the coil former instead of by a site pipefitter, and the whole heat-transfer surface fits into a fraction of the shell volume. The tighter, curved flow path also keeps the fluid turbulent at lower velocity, which raises the film coefficient and reduces the temperature gradient across the wall — the difference between a coil that reaches duty and one that runs 30 °C short of it.
ASTM A213 TP316L Stainless Steel Tube Coiled Tube Chemical Composition
| Grade | UNS Designation | C | M | P | S | Si | Ch | Ni | Mo | N | Nb | Ti | Other |
| TP316L | S31603 | 0.035 | 2 | 0.045 | 0.03 | 1 | 16.0–18.0 | 10.0–14.0 | 2.00–3.00 | ... | ... | ... | ... |
ASTM A213 TP316L Stainless Steel Tube Coiled Tube Mechanical properties
|
Grade
|
Tensile Str
(MPa) min |
Yield Str
0.2% Proof (MPa) min |
Elong
(% in 50mm) min |
Hardness
|
|
|
Rockwell B (HR B) max
|
Brinell (HB) max
|
||||
|
316L |
485
|
170
|
40
|
95
|
217
|
ASTM A213 TP316L Stainless Steel Tube Coiled Tube Physical Properties
|
Grade
|
Density
(kg/m3) |
Elastic Modulus
(GPa) |
Mean Co-eff of Thermal Expansion (m/m/0C)
|
Thermal Conductivity
(W/m.K) |
Specific Heat 0-1000C
(J/kg.K) |
Elec Resistivity
(nΩ.m) |
|||
|
0-1000C
|
0-3150C
|
0-5380C
|
At 1000C
|
At 5000C
|
|||||
|
316/L
|
8000 |
193
|
15.9
|
16.2
|
17.5
|
16.3
|
21.5
|
500 |
740 |
Technical FAQ
A site bend is only as good as the bender: ovality, wall thinning on the outside radius and residual stress all end up in the tube wall, and every joint between straight sections has to be welded and inspected. A factory coil is formed on a controlled former, annealed after forming and tested as a finished coil, so wall thinning and ovality are known values and the number of welds inside the equipment drops to two — inlet and outlet.
Not for raw, warm seawater. Chloride pitting and crevice attack on 316L become a real risk in seawater above roughly 60 °C, and stagnant seawater in a coil that is drained down only occasionally will crevice-corrode. 316L is the correct choice for treated, brackish or low-chloride cooling water, and for seawater only at low temperature with a strict velocity and cleaning regime. For raw warm seawater, a 6 % molybdenum grade or titanium tube should be evaluated instead.
Standard: chemical composition per heat, tensile and hardness, flattening and flaring, hydrostatic test and eddy-current test, all recorded per coil and summarised on an EN 10204 3.1 certificate. Optional: ASTM A262 Practice E intergranular corrosion test, positive material identification, ultrasonic or dye-penetrant test on the ends, third-party witness (ABS, GL, DNV, NK, CCS) and 3.2 certification.
Application
1. Heat exchanger coils and U-tube / hairpin bundles. Chemical, petrochemical and refinery exchangers running process streams that are aggressive to carbon steel but not chloride-saturated; the coil replaces a welded serpentine and removes the joints inside the shell.
2. Heating and cooling coils inside vessels. Internal coils in reactors, crystallisers, fermentation tanks and storage vessels, where the coil is installed through a manway in one piece and the surface area per unit volume decides the batch time.
3. Boiler, superheater and reboiler tubing. A213 is the tube specification written for boiler and heat-exchanger service, so the same tube covers superheater elements and reboiler bundles where creep and oxidation resistance matter.
4. Pharmaceutical, food and hygienic duty. CIP-cleaned coils, jacket and tank heating where a pickled and passivated, crevice-free bore is required and where copper alloys or mild steel are excluded by the cleaning regime.
5. Power generation and heat recovery. Auxiliary coolers, flue-gas and low-grade heat recovery coils, where a compact coil bank is easier to fit into an existing duct than a straight-tube bank.
6. Marine and offshore (with a chloride check). 316L is the practical choice for brackish, treated or low-chloride cooling water; for raw seawater at elevated temperature, a higher-molybdenum grade or titanium should be evaluated rather than assumed.
Overall Rating
Rating Snapshot
The following is the distribution of all ratingsAll Reviews