| Brand Name: | YUHONG |
| Model Number: | ASME SA192 Carbon Steel Boiler Tube |
| MOQ: | 1000kgs |
| Packaging Details: | Ply-wooden Case /Iron Case |
| Payment Terms: | L/C,T/T |
ASTM A192 / ASME SA192 Carbon Steel Boiler Tube Seamless Steel Boiler Tubing
Procurement Checklist
When ordering ASTM A192 bent boiler tubes, provide the following:
Quantity (pieces or meters)
OD and Wall Thickness (e.g., 50.8 mm x 5.0 mm)
Length (straight length or bent drawing)
Bending Details (radius, angle, plane, tolerances)
End Preparation (plain, beveled, threaded)
Certification Requirements (3.1, 3.2, or client-specific)
Packing
Comparison with Similar Grades
| Grade | Standard | Key Difference |
|---|---|---|
| ASTM A192 | Boiler Tubes | Low carbon, moderate strength, seamless |
| ASTM A106 Gr. B | Pipe for High Temp | Similar chemistry but for piping (larger sizes) |
| ASTM A179 | Heat Exchanger Tubes | Cold drawn, lower carbon, tighter tolerances |
| ASTM A210 Gr. A1 | Boiler Tubes | Higher carbon, higher strength |
| EN 10216-2 P235GH | European Standard | Comparable pressure vessel grade |
Chemical Composition % of ASTM A192 / ASME SA192 Carbon Steel Seamless Tube Boiler Tube Superheater Tube
|
Standard |
Chemical Compostion % |
||||
|---|---|---|---|---|---|
|
C |
Si |
Mn |
P |
S |
|
| ASTM A192 / ASME SA1920 | 0.06-0.18 | ≤0.25 | 0.27-0.63 | ≤0.035 | ≤0.035 |
Mechanical Properties of ASTM A192 / ASME SA192 Carbon Steel Seamless Tube Boiler Tube Superheater Tube
|
Hardness (HRB) |
Yield Strength (Mpa) |
Tensile Strength (Mpa) |
Elongation (%) |
|---|---|---|---|
| ≤77 | ≥180 | ≥325 | ≥35 |
Testing & inspection
Hydrostatic test OR nondestructive electric test is at the manufacturer’s option. If you require hydrostatic specifically, you must say so. Otherwise you may receive NDE only.
Flattening test is mandatory for A192. Flaring test is not required for A192, but it is required for A179. Dual-certified A179/A192 tubes will therefore have both.
No weld repairs. Because A192 is seamless, welding repair of defects is generally not permitted. Defective sections are cut off or rejected.
NDE method is not fixed. If NDE is used, the manufacturer may choose eddy current or ultrasonic. If you need a specific method, specify it.
Power plant boilers
Industrial boilers
Superheaters and reheaters
Water walls
Economizers
Heat exchangers